General purpose grade, high impact, high elongation, medium viscosityInformation provided by Asahi Kasei Corporation.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
Asahi Kasei Method
Melt Flow 10 g/10 min
10 g/10 min
ISO 1133 D
Mechanical Properties Metric English Comments
Tensile Strength at Break 72.0 MPa
10400 psi
ISO 527 - 1 & - 2
Elongation at Break 50 %
50 %
ISO 527 - 1 & - 2
Tensile Modulus 3.20 GPa
464 ksi
ISO 527 - 1 & - 2
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179 / 1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 165 °C
329 °F
ISO 75 -1 & -2 flat
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ISO 75 -1 & -2 flat
Flammability, UL94 HB
HB