Ashley Polymers Ashlene® 525-B2 Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 525-B2 Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A high impact modified lubricated nylon resin containing well dispersed carbon black for maximum resistance to weathering.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D785
Tensile Strength, Yield 55.0 MPa
7980 psi
ASTM D638
Elongation at Break 65 %
65 %
ASTM D638
Flexural Modulus 1.70 GPa
247 ksi
ASTM D790
Izod Impact, Notched 2.08 J/cm
3.90 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 249 °C
480 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 119 °C
246 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C
151 °F
ASTM D648