Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® 525LD-13G Nylon 66, 13% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 525LD-13G Nylon 66, 13% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High impact Nylon 66 reinforced with 13% glass fibers.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 93.0 MPa
13500 psi
ASTM D638
Elongation at Break 5.2 %
5.2 %
Flexural Modulus 3.80 GPa
551 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm
2.49 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 229 °C
444 °F
ASTM D648
Users viewing this material also viewed the following: