Ashley Polymers Ashlene® 527LD-45LG Nylon 66, 45% Long Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 50% Glass Fiber Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 527LD-45LG Nylon 66, 45% Long Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Long glass fiber reinforced impact modified Nylon 66, designed for parts requiring excellent thermal and dimensional stability and higher strength than available with conventional glass reinforced resins.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Ultimate 173 MPa
25100 psi
ATSM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Flexural Strength 216 MPa
31300 psi
ASTM D790
Flexural Modulus 7.90 GPa
1150 ksi
ASTM D790
Izod Impact, Notched 3.74 J/cm
7.01 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 252 °C
486 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 257 °C
495 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 253 °C
487 °F
ASTM D648