Ashley Polymers Ashlene® 539L Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced, Flame Retardant
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 539L Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High viscosity for injection molding of heavy parts.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 1.5 %
1.5 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 125
125
ASTM D785
Tensile Strength, Ultimate 81.0 MPa
11700 psi
ATSM D638
Elongation at Break 72 %
72 %
ASTM D638
Tensile Modulus 2.80 GPa
406 ksi
ASTM D638
Flexural Strength 113 MPa
16400 psi
ASTM D790
Flexural Modulus 2.50 GPa
363 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 257 °C
495 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 226 °C
439 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °C
165 °F
ASTM D648
Flammability, UL94 V-2
V-2
Users viewing this material also viewed the following: