Ashley Polymers Ashlene® 71M Nylon 6, 40% Mineral Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Mineral Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 71M Nylon 6, 40% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A 40% mineral reinforced Nylon 6 resin modified for reduced shrinkage.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ASTM D792
Water Absorption 1.1 %
1.1 %
ASTM D570
Moisture Absorption at Equilibrium 1.7 %
1.7 %
50% RH; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength, Yield 83.0 MPa
12000 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Modulus 5.40 GPa
783 ksi
ASTM D790
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 118 °C
244 °F
ASTM D648