Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® ABS R214

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® ABS R214.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Reprocessed for general purpose, general application, requiring good impact properties.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Melt Flow 1.5 g/10 min
1.5 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.0 MPa
5950 psi
ASTM D638
Tensile Modulus 2.241 GPa
325.0 ksi
ASTM D638
Izod Impact, Notched 2.14 J/cm
4.01 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 100 °C
212 °F
ASTM D1525