Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® P258 PPO

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, Molded
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® P258 PPO.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A high flow grade for applications requiring good impact strength and a high heat deflection temperature.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 1.06 g/10 min

@Load 3.80 kg,
Temperature 235 °C
1.06 g/10 min

@Load 8.38 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 48.0 MPa
6960 psi
ATSM D638
Elongation at Break 42 %
42 %
ASTM D638
Flexural Modulus 2.70 GPa
392 ksi
ASTM D790
Izod Impact, Notched 1.87 J/cm
3.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 181 °C
358 °F
ASTM D3418