Ashley Polymers Ashlene® P260WO PPO

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, Molded
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® P260WO PPO.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A general purpose V-0 rated resin with good impact strength.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Ultimate 48.0 MPa
6960 psi
ATSM D638
Flexural Modulus 2.20 GPa
319 ksi
ASTM D790
Izod Impact, Notched 2.83 J/cm
5.30 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
180 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in