Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® R190H2 Acetal

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® R190H2 Acetal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose economy grade copolymer, excellent toughness, strength, stiffness and lubricity. UV stabilized for maximum weatherability. Available in Natural and Black. Natural: Designated R190H2-N3; Black: Designated R190-H2B.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.022 cm/cm
0.022 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM D955
Melt Flow 8.0 - 10 g/10 min
8.0 - 10 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ATSM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Modulus 2.50 GPa
363 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ASTM D3418