Asia Technology Pioneers CAP 102 PP Nanocomposite

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Asia Technology Pioneers
Trade Name CAP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asia Technology Pioneers CAP 102 PP Nanocomposite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: CAP102 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective. Advantages:Good paint abilityGood dimensional (Heat) stabilityOutstanding surface appearanceUV resistanceGood Scratch resistanceCertification:ISO 9001:2008Iranian Nano Technology Initiative Council CertificationCertification from automakersApplication:Automotive Interior Parts (Dashboard Items)Automotive Exterior and Interior Paint-on PartsInformation provided by Asia Technology Pioneers
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Melt Flow 11.6 g/10 min

@Temperature 230 °C
11.6 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 37.3 MPa
5400 psi
ASTM D638M
Flexural Strength 43.08 MPa
6248 psi
ASTM D790
Flexural Modulus 0.206 GPa
29.9 ksi
ASTM D790
Izod Impact, Notched 0.382 J/cm
0.716 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Form Pellets - Tan color
Processing Method Injection Molding
Reinforcement Additives Nano Particles