Axiall 10801 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 10801 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Jacket compound recommended for 80°C maximum service temperature at a minimum wall thickness of 30 mils. UL recognized for 720 hour sunlight resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.43 - 1.47 g/cc
1.43 - 1.47 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 77 - 83
77 - 83
delayed; ASTM D-2240
Tensile Strength, Yield 13.4 MPa
1950 psi
ASTM D-638
Elongation at Yield 269.6 %
269.6 %
Air Aging: 240 hours @ 100°C; 30 mil slabs; UL 1581
330 %
330 %
ASTM D-638
100% Modulus 0.00689 GPa
1.00 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -24.0 °C
-11.2 °F
ASTM D-746
Oxygen Index 23 %
23 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 177 °C
350 °F