Material Notes:
Non-lead stabilized, UL recognized 720 hour sunlight resistant in all colors, 105 C rated jacket compound with good low temperature performance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 70 - 76
70 - 76
delayed; ASTM D-2240
Tensile Strength, Yield 16.5 MPa
2400 psi
ASTM D-638
Elongation at Yield 245.5 %
245.5 %
Air Aging: 7 days @ 136°C; 30 mil slabs; UL 1581
266.2 %
266.2 %
Oil Aging: 7 days @ 60°C; IRM 902 oil; 30 mil slabs; UL 1581
340 %
340 %
ASTM D-638
100% Modulus 0.00689 GPa
1.00 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -35.0 °C
-31.0 °F
ASTM D-746
Oxygen Index 25 %
25 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F