Material Notes:
Flame retarded CATV and general purpose jacket with excellent low temperature properties. UL approved for 720 hour sunlight resistance in all colors. UL approved for 94 V-0 at 1.5 mm in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 77 - 83
77 - 83
delayed; ASTM D-2240
84 - 90
84 - 90
ASTM D-2240
Tensile Strength, Yield 17.9 MPa
2600 psi
ASTM D-638
Elongation at Yield 252.8 %
252.8 %
Air Aging: 7 days @ 110°C; 75-mil plaques; UL 1581
320 %
320 %
ASTM D-638
100% Modulus 0.0107 GPa
1.55 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -42.0 °C
-43.6 °F
ASTM D-746
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
All colors
Oxygen Index 29 %
29 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F