Material Notes:
Georgia Gulf 6509 is a non-regulated, high flow, injection molding compound that has been specifically designed for outdoor applications that require an added degree of static resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D-785
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Tensile Modulus 2.41 GPa
350 ksi
ASTM D-638
Flexural Strength 75.8 MPa
11000 psi
ASTM D-790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D-790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm,
Temperature -20.0 °C
1.00 ft-lb/in

@Thickness 0.125 in,
Temperature -4.00 °F
ASTM D-256
7.47 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
14.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Gardner Impact 25.3 J

@Temperature 23.0 °C
18.7 ft-lb

@Temperature 73.4 °F
1/2" R Tup, 62 mil
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 74.00 °C
165.2 °F
ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D-648
Flammability, UL94 V-0
V-0
Oxygen Index 36 %
36 %
ASTM D-2863
Descriptive Properties Value Comments
Flow Ratio (Distance/Wall Thickness, 390-400°F) 215
Internal
Users viewing this material also viewed the following: