Axiall 8560 Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 8560 Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A clear, semi-rigid extrusion or molding grade compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.26 - 1.30 g/cc
1.26 - 1.30 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 53 - 59
53 - 59
delayed; ASTM D-2240
Tensile Strength, Yield 22.1 MPa
3200 psi
ASTM D-638
Elongation at Yield 275 %
275 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 188 °C
370 °F