Material Notes:
General purpose clear extrusion compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.22 - 1.26 g/cc
1.22 - 1.26 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 77 - 83
77 - 83
delayed; ASTM D-2240
Tensile Strength, Yield 17.6 MPa
2550 psi
ASTM D-638
Elongation at Yield 375 %
375 %
ASTM D-638
100% Modulus 0.00862 GPa
1.25 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -35.0 °C
-31.0 °F
ASTM D-746
Processing Properties Metric English Comments
Melt Temperature 179 °C
355 °F