Axiall 8864 Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 8864 Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose PVC extrusion compound recommended for applications that require UV and fungus resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.47 - 1.51 g/cc
1.47 - 1.51 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 83 - 89
83 - 89
delayed; ASTM D-2240
Tensile Strength, Yield 14.1 MPa
2050 psi
ASTM D-638
Elongation at Yield 320 %
320 %
ASTM D-638
100% Modulus 0.00848 GPa
1.23 ksi
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F