Axiall Suprel® SVA 9412 Rigid PVC, Molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name Suprel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall Suprel® SVA 9412 Rigid PVC, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf Suprel® SVA 9412 injection molding alloy features excellent impact resistance, excellent processing characteristics and comprehensive UL listings. The UL listings of Suprel 9412 include elevated Relative Thermal Index ratings, weatherability listings per UL 746C and good flammability listings.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.4 MPa
4700 psi
ASTM D-638
Tensile Modulus 1.93 GPa
280 ksi
ASTM D-638
Flexural Strength 50.3 MPa
7300 psi
ASTM D-790
Flexural Modulus 1.72 GPa
250 ksi
ASTM D-790
Izod Impact, Notched 1.60 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
3.00 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D-256
8.01 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D-256
Gardner Impact 0.102 J

@Thickness 1.59 mm,
Temperature -40.0 °C
0.0750 ft-lb

@Thickness 0.0625 in,
Temperature -40.0 °F
per mil; ASTM D-4226
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
unannealed; ASTM D-648
81.00 °C
177.8 °F
annealed; ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 66.00 °C
150.8 °F
unannealed; ASTM D-648
80.0 °C
176 °F
annealed; ASTM D-648
Vicat Softening Point 88.3 °C
191 °F
annealed; ASTM D-1525A
UL RTI, Electrical 95.0 °C
203 °F
UL-746B
UL RTI, Mechanical with Impact 85.0 °C
185 °F
UL-746B
UL RTI, Mechanical without Impact 95.0 °C
203 °F
UL-746B
Flammability, UL94 V-0

@Thickness 2.54 mm
V-0

@Thickness 0.100 in
5VA

@Thickness 2.00 mm
5VA

@Thickness 0.0787 in
Descriptive Properties Value Comments
UL Weatherability Rating F(1)/F(2)
UL-746C
Users viewing this material also viewed the following: