Material Notes:
Formula: C9H17ClO2CAS: 24468-16-1Description: 2-Ethylhexyl Chloroformate is a colorless to yellowish liquid with a pungent odor. It hydrolyzes in the presence of water.Synonyms: Chloroformic acid 2-ethylhexyl ester, Carbonochloridic acid, 2ethylhexyl esterApplications: Intermediate used in Plastics processing and Organic peroxide.Information provided by BASF
Physical Properties Metric English Comments
Density 0.988 g/cc
0.0357 lb/in³
Molecular Weight 192.7 g/mol
192.7 g/mol
Thermal Properties Metric English Comments
Melting Point <= -55.0 °C
<= -67.0 °F
Flash Point 87.0 °C
189 °F
Descriptive Properties Value Comments
Assay >99%
Color <25
APHA, DIN EN 1557
Composition 2-Ethylhexanol
<0.25%
Alkyl chloride
<0.03%
Bis(2ethylhexyl)carbonate
<0.5%
Fe
<5 ppm
HCl
<0.05%
Phosgene
<0.01%
Ignition Temperature 215°C