Material Notes:
Capron 8259 is a type 6 nylon injection molding graft copolymer developed for fastener applications requiring to abusive impact molding combined with a high level of pullout strength. It exhibits varying levels of toughness and flexibility combined with thermal and chemical resistance properties provided by the polyamide backbone.Capron 8259 is generally recommended for fastener applications.Data provided by Allied Signal.Processing: Max. water content 0.2%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.Melt Temperature: 240-270 degC (464-518 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) A mold temperature of 80-95 degC (176-203 degF) is recommended, but temperatures of as low as 10 degC (50 degF) can be used where applicable. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ISO data
Water Absorption 1.3 %
1.3 %
24 hrs; ISO data
Moisture Absorption at Equilibrium 2.0 %
2.0 %
50% RH; 23°C; ISO data
Water Absorption at Saturation 7.1 %
7.1 %
in water; 23°C; ISO data
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM Data MD
Mechanical Properties Metric English Comments
Tensile Strength, Yield 59.0 MPa
8560 psi
ISO value at 50 mm/min.
60.0 MPa
8700 psi
ASTM value at 50 mm/min.
Elongation at Break >= 100 %
>= 100 %
Nominal
Flexural Yield Strength 75.0 MPa
10900 psi
ASTM Data
Flexural Modulus 2.00 GPa
290 ksi
ASTM Data
Poissons Ratio 0.35
0.35
ISO data
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM and ISO test
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM Data
Processing Properties Metric English Comments
Drying Temperature 85.0 °C
185 °F
See Materials Notes