BASF Nypel® 6015G HS BK 15% Glass Filled PA6 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled
Manufacturer BASF
Trade Name Nypel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Nypel® 6015G HS BK 15% Glass Filled PA6 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nypel 6015G HS BK is a 15% glass reinforced, heat stabilized injection molding compound. It offers good mechanical properties with excellent processability.