Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer BASF
Trade Name Nypel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Nypel® RC6030F BK 30% Glass Filled PA6 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nypel® RC 6030F BK is a heat stabilized, 30% glass fiber reinforced injection molding grade.Application: Nypel® RC 6030F BK is generally recommended for applications such as bolts, racks, automotive underhood components, pressure regulator housings caps.Information provided by BASF