BASF Paliogen® Blue L 6385 Color Additive

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer BASF
Trade Name Paliogen®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Paliogen® Blue L 6385 Color Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Extreme reddish indanthrone blue pigment with excellent fastness propertiesPhysical form: PowderSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing systems, Amine curing systems, and Airdrying systems.Information provided by BASF