Material Notes:
Description: Pluracol® 4650 polyol is a secondary hydroxyl-terminated graft polyether triol containing approximately 44% solids of copolymerized styrene and acrylonitrile. This polyol has been formulated with a low volatile inhibitor package designed for either conventional curing or mechanical forced-air curing. This high solids graft polyol can be used to manufacture flexible slabstock foam having maximum load-bearing properties. It can be used alone for maximum effect or in combination with conventional polyols. Major applications for Pluracol 4650 include foams for prime carpet cushion, furniture seating and packaging. This polyol is a highly filtered version of Pluracol P4600.Information provided by BASF
Physical Properties Metric English Comments
Density 1.00 g/cc

@Temperature 40.0 °C
0.0361 lb/in³

@Temperature 104 °F
1.01 g/cc

@Temperature 25.0 °C
0.0365 lb/in³

@Temperature 77.0 °F
Viscosity 2160 cP

@Temperature 40.0 °C
2160 cP

@Temperature 104 °F
4340 cP

@Temperature 25.0 °C
4340 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.015
<= 0.015
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color White, Opaque Liquid
Hydroxyl Number 27 - 31 mg KOH/g
STI 3007/3162
Users viewing this material also viewed the following: