BASF Pluracol® 4800 HR Foam Polyol

Category Fluid
Manufacturer BASF
Trade Name Pluracol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Pluracol® 4800 HR Foam Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Pluracol® 4800 polyol is a primary OH tipped copolymer polyol containing approximately 45% copolymerized styrene-acrylonitrile suitable for molded foam applications. Pluracol polyol 4800 has been used in conjunction with Pluracol 1509 polyol to produce molded flexible foam that meets typical automotive specifications.Information provided by BASF
Physical Properties Metric English Comments
Density 1.04 g/cc

@Temperature 25.0 °C
0.0376 lb/in³

@Temperature 77.0 °F
1.04 g/cc

@Temperature 40.0 °C
0.0376 lb/in³

@Temperature 104 °F
Viscosity 3180 cP

@Temperature 40.0 °C
3180 cP

@Temperature 104 °F
7260 cP

@Temperature 25.0 °C
7260 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.015
<= 0.015
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color Creamy, Opaque Liquid
Hydroxyl Number 17 -21 mg KOH/g
STI 3007/3162