BASF Pluracol® 858 Specialty Polyol

Category Fluid
Manufacturer BASF
Trade Name Pluracol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Pluracol® 858 Specialty Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Pluracol® 858 polyol is a modifying polyol which can be used in a wide variety of applications. It can be employed as a cross-linking agent for rigid foam as well as coatings and elastomers. When combined with GP series polyols, high heat distortion resistant microcellular products can be produced.Information provided by BASF
Physical Properties Metric English Comments
Density 0.986 g/cc

@Temperature 43.4 °C
0.0356 lb/in³

@Temperature 110 °F
0.996 g/cc

@Temperature 32.2 °C
0.0360 lb/in³

@Temperature 90.0 °F
1.00 g/cc

@Temperature 25.0 °C
0.0361 lb/in³

@Temperature 77.0 °F
Viscosity 285 cP

@Temperature 43.4 °C
285 cP

@Temperature 110 °F
700 cP

@Temperature 32.2 °C
700 cP

@Temperature 90.0 °F
1360 cP

@Temperature 25.0 °C
1360 cP

@Temperature 77.0 °F
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color Clear Liquid
Hydroxyl Number 935 mg KOH/g
STI 3007/3162