BASF Ultramid® A3WG7 BK23210 35% Glass Filled PA66 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® A3WG7 BK23210 35% Glass Filled PA66 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ultramid A3WG7 BK23210 is a 35% glass fiber reinforced, pigmented black and heat resistance injection molding PA66 grade for machinery for industrial items.