Description: Impact-modified, 25% glass-fiber reinforced injection-molding grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; for components requiring high stiffness and enhanced toughness like photovoltaic connectors and junction boxes.Information provided by BASF