BASF Ultramid® B3WG6 CR BK 23210 15% Glass Filled (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® B3WG6 CR BK 23210 15% Glass Filled (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ultramid B3WG6 CR BK23210 s a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade for crash relevant applications.Information provided by BASF
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1138
Moisture Absorption at Equilibrium 2.1 %
2.1 %
50% RH; ISO 62
6.6 %
6.6 %
Saturation; ISO 62
Melt Flow 40.8 g/10 min

@Load 5.00 kg,
Temperature 275 °C
40.8 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 100 MPa
14500 psi
ISO 527
Elongation at Break 7.5 %
7.5 %
ISO 527
Tensile Modulus 5.60 GPa
812 ksi
ISO 527
Charpy Impact Unnotched 10.5 J/cm²
50.0 ft-lb/in²
ISO 179
Descriptive Properties Value Comments
Color BK 23210
Commercial Status North America