BASF Ultramid® C40 01 PA66/6 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, Unreinforced
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® C40 01 PA66/6 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ultramid C40 01 is a high viscosity, copolymer PA6/66 grade. Its very low melting point compared to standard PA6 is advantageous for coextrusion with temperature sensitive polymers like EVOH. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or legislations for other countries will be provided on request.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Water Absorption 10.5 %
10.5 %
ISO 62
Moisture Absorption at Equilibrium 3.2 %
3.2 %
23°C/50% R.H.; ISO 62
Relative Viscosity 4.0 cP
4.0 cP
ISO Test; 96 % SAV
Viscosity Test 250 cm³/g
250 cm³/g
Viscosity number
Thermal Properties Metric English Comments
Melting Point 190 °C
374 °F
10 K/min
Descriptive Properties Value Comments
Color Natural
Commercial Status North America and Europe
FDA 21 CFR 177.1500 (restrictions per 21 CFR .1395)
Impact Modified No
Primary Processing Technique Film Extrusion