Bapolan® 6055 Polystyrene, Injection Molding

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer Bapolan®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolan® 6055 Polystyrene, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolan PS6055 is a crystal polystyrene resin designed for injection molding applications requiring fast cycle times and superior optical properties. It complies with US FDA21 CFR177.1640 and 94HB UL rating.Applications: General purpose containers and cutlery.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers. All data is based on molded plaques.
Physical Properties Metric English Comments
Melt Flow 15 g/10 min
15 g/10 min
200'C/5,000g; ASTM D-1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Flexural Modulus, 1% Secant 3003 MPa
435500 psi
ASTM D-790A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °C
187 °F
ASTM D-648
Descriptive Properties Value Comments
Process Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution