Bapolene® PP5072 Polypropylene, Injection Grade

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Bapolene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® PP5072 Polypropylene, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolene PP 5072 is a multipurpose, high flow impact copolymer with excellent color and processability. This resin also exhibits a superior balance of stiffness and impact strength. This product meets the FDA requirements of 21CFR 177.1520.Applications: Containers, housewares, appliances, toys.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers.
Physical Properties Metric English Comments
Density 0.904 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Yield 26.9 MPa
3900 psi
50 mm/min (2 in./min.); ASTM D638
Elongation at Yield 5.0 %
5.0 %
50 mm/min (2 in./min.); ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
Secant @ 1% strain; ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C
210 °F
ASTM D648
Descriptive Properties Value Comments
Process Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved