Beijing Evergrow Resources ACFC1750 Activated Carbon Fiber Cloth

Category Carbon , Carbon Fiber
Manufacturer Beijing Evergrow Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Evergrow Resources ACFC1750 Activated Carbon Fiber Cloth.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Properties:High adsorption speed capacityGood efficiency towards pesticides and odorsPossible adaptation to condition of useHigh voluminal adsorption capacityRegenerableLow mineral content Applications:Solvent recoveryAir purificationWater purificationDecoloring of liquidDeodoring in refrigeraterSanitary productsNBC protection suitsWound care productsInformation provided by Beijing Evergrow Resources.
Physical Properties Metric English Comments
Specific Surface Area 1750 m²/g
1750 m²/g
BET
Descriptive Properties Value Comments
Area Density 95-105 g/m²
Pore Volume (ml/g) 0.8-0.9
Width (mm) 750-850