Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Beijing Evergrow Resources PTFE Adhesive Tape

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Beijing Evergrow Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Evergrow Resources PTFE Adhesive Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PTFE adhesive tape is manufactured by PTFE high strength suspension resin. The skived PTFE tape is one side etched, and then coated with adhesive back and chippd to different sizes. It is anticorrosive, insulative and does not age. PTFE Adhesive Tape is widely used in the fields that PVC does not apply to. Applications: Covers for high performance cables and wires; also covers for cables and wires in high qualified places like hotels, big marketplaces, entertainment places and gymnasiums, etc; covers for cables and wires in open country; sealing for mechanical packers.Information provided by Beijing Evergrow Resources.
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 25.0 MPa
>= 3630 psi
Elongation at Break 125 %
125 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 10.0 kV/mm
>= 254 kV/in
Descriptive Properties Value Comments
Adhesive Bond Strength (N/25mm) 6