Beijing Ranger Chem SM-601 Solid Epoxy Resin

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Beijing Ranger Chemical Co
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Ranger Chem SM-601 Solid Epoxy Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Beijing Ranger Chemical Co.
Physical Properties Metric English Comments
Volatiles <= 5.0e-7 %
<= 5.0e-7 %
Thermal Properties Metric English Comments
Softening Point 60.0 - 76.0 °C
140 - 169 °F
Optical Properties Metric English Comments
Gardner Color Number <= 0.50
<= 0.50
Descriptive Properties Value Comments
Epoxy Equivalent g/eq 450-560
Inorganic Chlorine ppm, = 5
Saponifiable Chlorine ppm, = 300
Total Chlorine ppm, = 1400