Beijing Ranger Chem SM-828X80 Solvent Based Epoxy Resin

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Beijing Ranger Chemical Co
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Ranger Chem SM-828X80 Solvent Based Epoxy Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Beijing Ranger Chemical Co.
Physical Properties Metric English Comments
Solids Content 79 - 81 %
79 - 81 %
Viscosity 50 - 200 cP
50 - 200 cP
Optical Properties Metric English Comments
Gardner Color Number <= 0.20
<= 0.20
Descriptive Properties Value Comments
Epoxy Equivalent g/eq 184-194
Inorganic Chlorine ppm, = 5
Saponifiable Chlorine ppm, = 100
Solvent Xylene
Total Chlorine ppm, = 1400