Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name Borclear™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borclear™ RE936CF Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borclear™ RE936CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: food packaging, lamination films, and stationary films. Additives: Borclear™ RE936CF contains antiblock and slip agents.Information provided by Borealis AG
Physical Properties Metric English Comments
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Slip Level 2000 ppm
2000 ppm
EAA; Borealis Method
Mechanical Properties Metric English Comments
Tensile Modulus 0.500 GPa
72.5 ksi
MD/TD; ISO 527-3
Flexural Modulus 0.900 GPa
131 ksi
ISO 178
Dart Drop, Total Energy 20.0 J
14.8 ft-lb
1000N; ISO 7765-1
Coefficient of Friction 0.15
0.15
film to film; ISO 8295
Film Tensile Strength at Break, MD 30.0 MPa
4350 psi
ISO 527-3
Film Tensile Strength at Break, TD 30.0 MPa
4350 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 143 °C
289 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 66.0 °C
151 °F
ISO 75-2
Vicat Softening Point 130 °C

@Load 1.02 kg
266 °F

@Load 2.25 lb
A50; ISO 306
Optical Properties Metric English Comments
Haze <= 1.5 %
<= 1.5 %
ASTM D1003
Gloss 140 %
140 %
20° of arc; ASTM D2457
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Component Elements Properties Metric English Comments
SiO2 0.18 %
0.18 %
Borealis Method