Brandenburger BRA-FLEX Side Insulation

Category Polymer , Thermoset , Filled/Reinforced Thermoset
Manufacturer Brandenburger
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Brandenburger BRA-FLEX Side Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Brandenburger Isoliertechnik GmbH&Co.
Mechanical Properties Metric English Comments
Compressive Strength 1.00 MPa
145 psi
EN ISO 604
1.00 MPa

@Temperature 200 °C
145 psi

@Temperature 392 °F
EN ISO 604
Thermal Properties Metric English Comments
Thermal Conductivity 0.0600 W/m-K
0.416 BTU-in/hr-ft²-°F
DIN 52 612
Maximum Service Temperature, Air 280 °C
536 °F
Long Term
Descriptive Properties Value Comments
Chemical Resistance oil, petrol, lubricants, aqueous solutions, diluted acids and lyes