Description: Injection Molding, General Purpose, Low Water Carryover, UV ResistantApplications: Suggested Uses Include Tape, Slit-film Fibers, Containers, Closures, HousewaresThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDAInformation provided by Braskem
Physical Properties Metric English Comments
Melt Flow 4.2 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.2 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
ASTM D785
Tensile Strength 37.2 MPa
5400 psi
2 in/min; ASTM D638
Elongation at Yield 10 %
10 %
2 in/min; ASTM D638
Tenacity 0.397 N/tex
4.50 g/denier
3.3 draw ration, 1,250 m/min roll speed; 225°C spin temperature, D1000/68, ASTM D2256
Flexural Modulus 1.59 GPa
230 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256A
Descriptive Properties Value Comments
Elongation of Fibers (3.3 draw ration, 1,250 m/min roll speed) 36%
225°C spin temperature, D1000/68, ASTM D2256
Users viewing this material also viewed the following: