Material Notes:
Description: Superior Antistatic properties, excellent mold release.Applications: Suggested uses include closures, housewares.Process: Injection Molding.This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Tensile Strength 37.2 MPa
5400 psi
2 in/min; ASTM D638
Elongation at Yield 9.0 %
9.0 %
2 in/min; ASTM D638
Flexural Modulus 1.59 GPa
230 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256A