Material Notes:
Description: Maximum see-through clarity, minimal haze; superior color stability, process stability and gloss. Applications: Suggested uses include extrusion, blow molding, thermoforming, food containers, packaging. Ultraclear (TM) polypropylene resin offers great clarity and performance, up to 50% improvement in haze over standard clarified products. If offers substitution opportunities versus more expensive resins such as PET, PVC, PC or PS. Process: Blow Molding. This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by FDA – Food and Drugs Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 30.3 MPa
4400 psi
2 in/min; ASTM D638
Elongation at Yield 13 %
13 %
2 in/min; ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
ASTM D256A
Optical Properties Metric English Comments
Haze 5.0 %
5.0 %
50 mil Disc; ASTM D1003
Users viewing this material also viewed the following: