CIMBAR FlexTalc® 1222D Ultrafine Talc for TPO Applications, Densified

Category Ceramic , Oxide , Silicon Oxide , Other Engineering Material , Additive/Filler for Polymer
Manufacturer CIMBAR Performance Minerals
Trade Name FlexTalc®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CIMBAR FlexTalc® 1222D Ultrafine Talc for TPO Applications, Densified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cimbar Performance Minerals' FlexTalc® products are an ultrafine talc product line specifically engineered for use in high performance TPO applications. FlexTalc® products are made by a proprietary process that results in talc products which have very high aspect ratios, are easily dispersed, provide heat aging and offer compounded color. They are available in powder and densified (D) forms.Information provided by Cimbar Performance Minerals.
Physical Properties Metric English Comments
Specific Gravity 2.78 g/cc
2.78 g/cc
Brightness 65 %
65 %
wet
94 %
94 %
Hunter Rd, dry
Oil Absorption 58 %
58 %
g oil/100 g filler; ASTM D281
Moisture Absorption at Equilibrium 0.50 %
0.50 %
Loss On Ignition 7.5 %
7.5 %
Particle Size 2.5 µm
2.5 µm
D50
<= 11 µm
<= 11 µm
PSD 98%
pH 8.7
8.7
Component Elements Properties Metric English Comments
Al2O3 <= 1.0 %
<= 1.0 %
CaO <= 1.0 %
<= 1.0 %
Fe2O3 <= 1.0 %
<= 1.0 %
MgO 30 %
30 %
SiO2 60 %
60 %