C.O.I.M. DIEXTER® G172 Polyol Polyester

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyester, TP
Manufacturer C.O.I.M. S.p.A.
Trade Name DIEXTER®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF C.O.I.M. DIEXTER® G172 Polyol Polyester.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virtually every field of application. These saturated polyester resins can be used in applications ranging from the production of slab stocks to synthetic leathers and thermoplastics. Basic Composition = DEGInformation provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Viscosity 7300 - 8300 cP

@Temperature 35.0 °C
7300 - 8300 cP

@Temperature 95.0 °F
Molecular Weight 2800 g/mol
2800 g/mol
Descriptive Properties Value Comments
Hydroxyl Number (mg KOH/gr) 38
Min
42
Max
Structure linear