C.O.I.M. FILCO® 339 Film Former for Glass Fiber Sizes

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer C.O.I.M. S.p.A.
Trade Name FILCO®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF C.O.I.M. FILCO® 339 Film Former for Glass Fiber Sizes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and are collectively known as FILCO®. The products in the FILCO® line serve to size glass fiber, to optimize the mechanical characteristics of the fiber, or to bind the fibers for the production of mat.Typical Physical and Chemical Characteristics: Filco 339 is an unsaturated polyester-epoxy polymer in non-ionic water emulsionCharacteristics of the dried film: clearnot tackycompatible with unsaturated polyester and epoxy resinsvery quickly soluble in styreneApplications: Filco 339 is suggested as a film former for glass fiber sizes for:roving for translucent sheetspray rovingmat rovingFiber glass sized with Filco 339 present high impregnation speed during glass resin composite high transparency.Information provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Solids Content 52 - 56 %
52 - 56 %
MA145LFE
Particle Size 0.25 - 0.50 µm
0.25 - 0.50 µm
MA147LFE
pH 6.0 - 7.5
6.0 - 7.5
MA148LFE
Descriptive Properties Value Comments
Appearance Milky Liquid
Epoxy Equivalent on Dry Resin 220-280
(g), MA149LFE