C.O.I.M. FILCO® 354 N Unsaturated Bisphenolic Polyester Polymer for Glass Fiber Sizing

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer C.O.I.M. S.p.A.
Trade Name FILCO®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF C.O.I.M. FILCO® 354 N Unsaturated Bisphenolic Polyester Polymer for Glass Fiber Sizing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Unsaturated Bisphenolic Polyester Polymer for Glass Fiber SizingGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and are collectively known as FILCO®. The products in the FILCO® line serve to size glass fiber, to optimize the mechanical characteristics of the fiber, or to bind the fibers for the production of mat.Applications: Filco 354 N has been studied as a primary film forming component of glass fiber sizing for unsaturated polyester matrix strengthening. Consider the following special properties:good solubility in vinylic solventsgood compatibility with other typical sizing component formulationsgood compatibility and wet ability with various unsaturated polyester matrixesgood transparency of reinforced compositeshigh impregnation speed of sized fibers during glass/resin composites workingIt is recommendable to use Filco 354 N in combination with metacrylic radical organosilanes for glass fiber sizing formulation for:roving for translucent sheetsroving for weavingroving for chop/spraychopped strand mat with powder and liquid binder highly soluble in styreneInformation provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Solids Content 45 - 49 %
45 - 49 %
Particle Size 0.60 - 0.80 µm
0.60 - 0.80 µm
pH 2.5 - 4.5
2.5 - 4.5
Brookfield Viscosity 1.0 - 3.0 cP

@Temperature 20.0 °C
1.0 - 3.0 cP

@Temperature 68.0 °F
Brookfield RVT spindle 2.2 RPM
Descriptive Properties Value Comments
Appearance Milky Liquid