C.O.I.M. LARIPUR® LPR9025 Special Adipate Ester Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyester Thermoplastic Elastomer , Polyurethane, TP
Manufacturer C.O.I.M. S.p.A.
Trade Name Laripur®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF C.O.I.M. LARIPUR® LPR9025 Special Adipate Ester Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion resistanceGreat flexibility with constancy at temperature variationsGood compression resistanceGood water and light resistanceGood resistance to oils, fats and to many types of solventsSeries 25 Special Adipate Ester: These products are based on saturated polyesters. Products are based on saturated polyester. The features are similar to those of Series 20 but, by comparison, they are characterized by a higher resistance to hydrolysis and improved flexibility at low temperatures. Information provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Tensile Strength, Yield 60.1 MPa
8720 psi
ASTM D412
Elongation at Break 540 %
540 %
ASTM D412
50% Modulus 0.00580 GPa
0.841 ksi
ASTM D412
100% Modulus 0.00730 GPa
1.06 ksi
ASTM D412
300% Modulus 0.0241 GPa
3.50 ksi
ASTM D412
Tear Strength 106 kN/m
605 pli
ASTM D624
Abrasion 30
30
mm3, Abrasion Loss; DIN 53516
Compression Set 24 %
24 %
70 hours at 23°C; ASTM D395
45 %

@Temperature 70.0 °C
45 %

@Temperature 158 °F
Method B, 22 hours; ASTM D395
Thermal Properties Metric English Comments
Vicat Softening Point 104 °C
219 °F
ASTM D1525