Material Notes:
Description: Used in the fields of cable and fuel pipe manufacturing.Information provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Viscosity 1700 - 2700 cP

@Temperature 35.0 °C
1700 - 2700 cP

@Temperature 95.0 °F
Dynamic viscosity
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
Tensile Strength, Yield 25.14 MPa
3646 psi
Elongation at Break 271 %
271 %
100% Modulus 0.00876 GPa
1.27 ksi
Optical Properties Metric English Comments
Gardner Color Number 3.0
3.0
Chemical Properties Metric English Comments
Acid Value 2.0
2.0
mgKOH/g
Descriptive Properties Value Comments
Efficiency concentration PHR 39
N OH value (max) 35
mg KOH/g