Material Notes:
Cathay engineering polyamides contain 26-100% renewably sourced material. Advantages: Operates at similar conditions to PA66; Suitable for injection, compounding and extrusion; Stable mechanical propertiesInformation provided by Cathay
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ISO 1183
Water Absorption 0.20 %
0.20 %
ISO 62
4.6 %
4.6 %
Equilibrium, 50%RH; ISO 62
Water Absorption at Saturation 16 %
16 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 81.0 MPa
11700 psi
ISO 527-2
Elongation at Yield 4.9 %
4.9 %
ISO 527-2
Tensile Modulus 3.10 GPa
450 ksi
ISO 527-2
Flexural Strength 108 MPa
15700 psi
ISO 178
Flexural Modulus 2.65 GPa
384 ksi
ISO 178
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
ISO 180/1U
Charpy Impact Unnotched NB
NB
ISO 179/1eA
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 205 °C
401 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 67.5 °C
154 °F
ISO 75-2/A
Vicat Softening Point 217 °C
423 °F
ISO 306
Flammability, UL94 V-2

@Thickness 0.710 mm
V-2

@Thickness 0.0280 in
Oxygen Index 34.7 %
34.7 %
ISO 4589-2
Glow Wire Test 960 °C

@Thickness 1.50 mm
1760 °F

@Thickness 0.0591 in
IEC 60695-2-12