Material Notes:
Features:high puritycorrosion resistancewear resistanceApplications:semiconductor componentssputtering targetsInformation provided by Ceradyne Company
Physical Properties Metric English Comments
Density 3.15 g/cc
0.114 lb/in³
Weibull Modulus 12
12
Mechanical Properties Metric English Comments
Vickers Microhardness 2300
2300
0.3
Modulus of Elasticity 400 GPa
58000 ksi
Flexural Strength 380 MPa

@Temperature 23.0 °C
55100 psi

@Temperature 73.4 °F
Poissons Ratio 0.17
0.17
Fracture Toughness 2.50 MPa-m½
2.28 ksi-in½
Shear Modulus 171 GPa
24800 ksi
calculated
Abrasion 947
947
Abrasive Wear Resistance Parameter
Thermal Properties Metric English Comments
CTE, linear 4.80 µm/m-°C

@Temperature 20.0 - 1000 °C
2.67 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 115 W/m-K
798 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
Descriptive Properties Value Comments
Purity, % 99.3
Thermal Shock Parameter 164°C